Hi Mike,

The plating is gradually reduced throughout the tapered sections fore and aft to 16 mm (from 18 mm in midship).


>> Any idea where the platinum would come from?

I have not found the platinium in U864 cargo manifest, but maybe (along with mercury) it has been transfered to Japan as a cargo? It could be used as a alloying addition while manufacturing jet engines.

--
Regards
Maciek


[www.tvre.org]

Options: ReplyQuote


Subject Written By Posted
Use of metals in U boat pressure hulls wreckferret 03/16/2013 06:51PM
Re: Use of metals in U boat pressure hulls Simon 03/16/2013 07:10PM
Re: Use of metals in U boat pressure hulls SnakeDoc 03/17/2013 07:40PM
Re: Use of metals in U boat pressure hulls Scott Sorenson 03/18/2013 12:43AM
Re: Use of metals in U boat pressure hulls zakarpatska 03/18/2013 12:55PM


Your Name: 
Your Email: 
Subject: 
Spam prevention:
Please, enter the code that you see below in the input field. This is for blocking bots that try to post this form automatically.
 ********   ********   ********  **     **  ******** 
 **     **  **     **     **     **     **  **       
 **     **  **     **     **     **     **  **       
 **     **  ********      **     **     **  ******   
 **     **  **     **     **     **     **  **       
 **     **  **     **     **     **     **  **       
 ********   ********      **      *******   ********